 1. White spots

① White spots; a water-based protective agent was used on high-density stone because the surface was not cleaned in time. The protective agent causes white spots, which often appear on black granite. Sometimes it can happen to other stones or even singeing boards due to incorrect usage. The mixture is found to be white silicone resin and carbonate, which is difficult to remove with ordinary cleaners.

Solution: You can try to use the original Jinshite water-based protective agent on the surface and wipe it off with a stainless steel wire ball. This is useful on stone surfaces where white spots can be removed. If white spots appear on the burning board, it will be more troublesome. Use a hard-bristled brush to brush them off (sometimes not all of them can be brushed off). Whether you use steel wool or a hard-bristled brush, you must promptly remove stains on the brush and wipe with a towel dipped in water, otherwise traces will still be left.

You can also use a pre-dispersed protective agent, mixed with more than 5 times of ethanol, and clean it according to the above construction method after the heat generation phenomenon is completed. Pay attention to fire prevention and remove surface residues.

2. Grease-like flower marks

Reasons for occurrence: This phenomenon usually It happened when there was water inside the stone and Jinshite oil-based protective agent was used, forming oily stains. Or after using a water-based care agent, the stones are stacked together without waiting to dry, forming uneven patterns.

When the oil stain-like pattern is not serious, you can use stone degreaser and directly apply the degreaser evenly to the stone. The degreaser will Make the stains disappear; when the phenomenon is severe, apply degreasing ointment to allow dissipation and adsorption to proceed at the same time. When dealing with black pockmarked stone, you should be careful not to leave the white powder after the paste is dried on the surface of the stone.

3. Rust spots and yellow spots

Cause: rust spots and organic yellow spots appeared on the stone after using protective agent. There are pure water spots, and the surface of the stone has the effect of a hydrophobic protective agent, so that all potions cannot enter the stone and cannot remove pollution. This situation occurs more frequently on siliceous sandstone.

There are generally two methods: one is to use degreaser or protective agent remover, and use these cleaning agents to remove the solidified protective agent; Another option is to use a penetrating agent to moisten the surface of the stone, and then use a stone cleaning agent targeted at lesions to clean the stone.

AAADF3RSEGDTHIU


Disclaimer:

Disclaimer: Some of the texts, pictures, audios, and videos of some articles published on this site are from the Internet and do not represent the views of this site. The copyrights belong to the original authors. If you find that the information reproduced on this website infringes upon your rights, please contact us and we will change or delete it as soon as possible.

AA

This article is from the Internet, does not represent 【www.china-garment.com】 position, reproduced please specify the source.https://www.china-garment.com/archives/34238

Author: clsrich

 
TOP
Home
News
Product
Application
Search